Molds & Tooling 5 görüntüleme

Solution for mold temperature of calcium-zinc stabilizer in pipe production

Sorun Belirtisi
The calcium-zinc PVC system shows mold temperature-related abnormalities in the pipe production production stage, product quality is unstable.
Neden Analizi
The zinc burning characteristic of calcium-zinc stabilizers produces mold temperature problems under specific working conditions.
Çözüm
From the formulation perspective, reduce lubrication, combined with process optimization to solve it.
Temel Çıkarım
The mold temperature problem of the calcium-zinc system in the pipe production stage requires coordinated optimization of formulation and process.