Control of demolding abnormality in PEOX blown film laundry pods
Sorun Belirtisi
During PEOX blown film production of laundry pods, the problem of not up to standard demolding occurs.
Neden Analizi
Mainly due to the processing temperature deviating from the window +70-90°C, moisture content >0.5% exceeding the standard, and insufficient cooling.
Çözüm
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and shorten the residence time.
Temel Çıkarım
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.