Problembeschreibung
During PEOX blown film production of laundry pods, the problem of not up to standard demolding occurs.
Ursachenanalyse
Mainly due to the processing temperature deviating from the window +70-90°C, moisture content >0.5% exceeding the standard, and insufficient cooling.
Lösung
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and shorten the residence time.
Wichtigste Erkenntnis
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.