Material Drying
5 görüntüleme
Control of demolding abnormality in PEOX blown film pharmaceutical films
Sorun Belirtisi
During PEOX blown film production of pharmaceutical films, the problem of large fluctuation in demolding occurs.
Neden Analizi
Mainly due to the processing temperature deviating from the window +60-100°C, moisture content >0.1% exceeding the standard, and insufficient cooling.
Çözüm
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and strengthen cooling.
Temel Çıkarım
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.