Material Drying 2 views

Control of demolding abnormality in PEOX blown film pharmaceutical films

Problem Phenomenon
During PEOX blown film production of pharmaceutical films, the problem of large fluctuation in demolding occurs.
Cause Analysis
Mainly due to the processing temperature deviating from the window +60-100°C, moisture content >0.1% exceeding the standard, and insufficient cooling.
Solution
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and strengthen cooling.
Key Takeaway
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.