POE toughness insufficient, brittle fracture
Sorun Belirtisi
POE product elongation at break <50%, brittle fracture without yielding
Neden Analizi
POE molecular weight low, toughness foundation insufficient; excessive crosslinking loses toughness; coarse crystallization increases brittleness
Çözüm
1) Select high molecular weight POE to improve toughness; 2) Control crosslinking degree to avoid excess; 3) Nucleating agent to refine crystallization and improve toughness
Temel Çıkarım
Insufficient toughness is caused by low molecular weight and coarse crystallization; selecting high MW is key