Material Analysis 11 visualizaciones

POE toughness insufficient, brittle fracture

Fenómeno del problema
POE product elongation at break <50%, brittle fracture without yielding
Análisis de la causa
POE molecular weight low, toughness foundation insufficient; excessive crosslinking loses toughness; coarse crystallization increases brittleness
Solución
1) Select high molecular weight POE to improve toughness; 2) Control crosslinking degree to avoid excess; 3) Nucleating agent to refine crystallization and improve toughness
Conclusión clave
Insufficient toughness is caused by low molecular weight and coarse crystallization; selecting high MW is key
POEtoughness insufficientmolecular weightcrosslinking controlcrystallization refinement