Production & Quality 8 görüntüleme

POE internal inclusions

Sorun Belirtisi
POE product interior 0.1-0.5mm inclusions, affecting appearance
Neden Analizi
Impurity particles in raw material; production environment dust contamination; foreign matter mixed into recycled material
Çözüm
1) Raw material filtration with 120 mesh screen to remove impurities; 2) Production environment cleanliness, control dust; 3) Recycled material strictly sorted to remove foreign matter
Temel Çıkarım
Inclusions are caused by raw material and environmental contamination; filtration and environmental control are key