Production & Quality 5 visualizações

POE internal inclusions

Fenómeno do problema
POE product interior 0.1-0.5mm inclusions, affecting appearance
Análise das causas
Impurity particles in raw material; production environment dust contamination; foreign matter mixed into recycled material
Solução
1) Raw material filtration with 120 mesh screen to remove impurities; 2) Production environment cleanliness, control dust; 3) Recycled material strictly sorted to remove foreign matter
Conclusão principal
Inclusions are caused by raw material and environmental contamination; filtration and environmental control are key
POEinclusionsraw material filtrationenvironment cleanlinessrecycling sorting