Injection Molding 5 görüntüleme

Gate clogging of PET injection mold

Sorun Belirtisi
The gate frequently clogs during PET '2079851475616104452, injection pressure rises abnormally, and production is interrupted.
Neden Analizi
PET cools, crystallizes and solidifies too fast at the gate; gate size is too small; mold temperature in the gate area is on the low side.
Çözüm
Increase gate size; increase mold temperature in the gate area to 140-160°C; use a hot runner system.
Temel Çıkarım
The fast crystallization characteristic of PET easily causes gate clogging and needs to be addressed through mold temperature and gate design.