Extrusion & Post 5 görüntüleme

PETG poor adhesion during printing

Sorun Belirtisi
The ink adhesion on the PETG product surface is insufficient, easily peeling off or being scratched.
Neden Analizi
PETG surface energy is low (about 30-36mN/m), the surface has mold release agent or oil contamination residue, and the ink system does not match.
Çözüm
Corona treat the product surface to a dyne value ≥42mN/m; clean with alcohol before printing; select an ink system suitable for polyester.
Temel Çıkarım
PETG printing adhesion depends on surface treatment and ink matching.
PETGprintingadhesioncorona treatmentsurface energy