Extrusion & Post 8 visualizaciones

PETG poor adhesion during printing

Fenómeno del problema
The ink adhesion on the PETG product surface is insufficient, easily peeling off or being scratched.
Análisis de la causa
PETG surface energy is low (about 30-36mN/m), the surface has mold release agent or oil contamination residue, and the ink system does not match.
Solución
Corona treat the product surface to a dyne value ≥42mN/m; clean with alcohol before printing; select an ink system suitable for polyester.
Conclusión clave
PETG printing adhesion depends on surface treatment and ink matching.
PETGprintingadhesioncorona treatmentsurface energy