Production & Quality 5 görüntüleme

PETG product toughness decline at low temperature

Sorun Belirtisi
In use environments below 0°C, the impact strength of PETG products decreases significantly and they become brittle.
Neden Analizi
At low temperature, the movement of PETG molecular chain segments is restricted and there is a low-temperature embrittlement tendency; internal stress in the product aggravates low-temperature brittleness.
Çözüm
Design the product to avoid notches and sharp corners; increase mold temperature to reduce internal stress; use toughened modified grades if necessary.
Temel Çıkarım
PETG low-temperature toughness is better than PET, but product design and internal stress management still need attention.
PETGlow temperatureembrittlementtoughnessinternal stress

Bu faydalı oldu mu?

0 kişi bunu faydalı buldu

ChemAI