Production & Quality
6 مشاهدة
PETG product toughness decline at low temperature
ظاهرة المشكلة
In use environments below 0°C, the impact strength of PETG products decreases significantly and they become brittle.
تحليل الأسباب
At low temperature, the movement of PETG molecular chain segments is restricted and there is a low-temperature embrittlement tendency; internal stress in the product aggravates low-temperature brittleness.
الحل
Design the product to avoid notches and sharp corners; increase mold temperature to reduce internal stress; use toughened modified grades if necessary.
الخلاصة الأساسية
PETG low-temperature toughness is better than PET, but product design and internal stress management still need attention.