Injection Molding 5 görüntüleme

PETG '2079851475616104452 improper back pressure setting, poor plasticization

Sorun Belirtisi
Plasticization is uneven, with unmelted particles in the melt or insufficient mixing.
Neden Analizi
Back pressure too low, mixing and plasticization insufficient; back pressure too high increases shear heat and degradation risk.
Çözüm
Optimize back pressure setting to 0.5-1.5MPa; adjust according to plasticization quality and regrind condition.
Temel Çıkarım
PETG back pressure setting needs to balance plasticization quality and degradation risk.