Injection Molding
2 views
PETG '2079851475616104452 improper back pressure setting, poor plasticization
Problem Phenomenon
Plasticization is uneven, with unmelted particles in the melt or insufficient mixing.
Cause Analysis
Back pressure too low, mixing and plasticization insufficient; back pressure too high increases shear heat and degradation risk.
Solution
Optimize back pressure setting to 0.5-1.5MPa; adjust according to plasticization quality and regrind condition.
Key Takeaway
PETG back pressure setting needs to balance plasticization quality and degradation risk.