Injection Molding
5 görüntüleme
Insufficient shot amount of PETG '2079851475616104452
Sorun Belirtisi
The screw storage amount is insufficient to fill the cavity, and the product is incomplete.
Neden Analizi
The metering stroke setting is insufficient, the melt amount in the barrel is not enough, and the raw material density fluctuates.
Çözüm
Increase the metering stroke to ensure storage amount > injection amount *1.05; check the feeding stability.
Temel Çıkarım
For insufficient shot amount of PETG, ensure that the storage amount is always sufficient.
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu