Injection Molding
7 visualizações
Insufficient shot amount of PETG '2079851475616104452
Fenómeno do problema
The screw storage amount is insufficient to fill the cavity, and the product is incomplete.
Análise das causas
The metering stroke setting is insufficient, the melt amount in the barrel is not enough, and the raw material density fluctuates.
Solução
Increase the metering stroke to ensure storage amount > injection amount *1.05; check the feeding stability.
Conclusão principal
For insufficient shot amount of PETG, ensure that the storage amount is always sufficient.
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!