Material Drying
5 görüntüleme
Silver streaks and bubbles in PMMA '2079851475616104452
Sorun Belirtisi
Silver streaks and bubbles appear in PMMA transparent products.
Neden Analizi
PMMA has strong hygroscopicity (water absorption rate 0.3%); insufficient drying leaves moisture >0.05%, and moisture vaporizes at processing temperature producing silver streaks and bubbles.
Çözüm
Dry at 70-85°C for 4-6h to moisture <0.05%; use a dehumidifying dryer with dew point ≤-25°C.
Temel Çıkarım
PMMA drying is the first priority for transparent quality.
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu