Material Drying 3 Aufrufe

Silver streaks and bubbles in PMMA '2079851475616104452

Problembeschreibung
Silver streaks and bubbles appear in PMMA transparent products.
Ursachenanalyse
PMMA has strong hygroscopicity (water absorption rate 0.3%); insufficient drying leaves moisture >0.05%, and moisture vaporizes at processing temperature producing silver streaks and bubbles.
Lösung
Dry at 70-85°C for 4-6h to moisture <0.05%; use a dehumidifying dryer with dew point ≤-25°C.
Wichtigste Erkenntnis
PMMA drying is the first priority for transparent quality.
PMMAsilver streakbubbledryingmoisture