Poor thermal stability of styrene-butadiene transparent resin (K resin) during processing

Sorun Belirtisi
Styrene-butadiene transparent resin (K resin) has poor thermal stability during processing; performance decreases significantly after repeated processing, with severe degradation
Neden Analizi
Insufficient antioxidant addition or improper type Processing temperature too high (exceeding the 200-240°C upper limit) accelerates degradation Excessive screw shear accelerates thermo-oxidative degradation Regrind ratio too high, degradation accumulates Antioxidants fail at high temperature
Çözüm
Increase antioxidant addition amount Reduce processing temperature to a reasonable value of 200-240°C Reduce screw rotation speed to reduce shear Reduce regrind ratio ≤15% Select antioxidants with good high-temperature stability
Temel Çıkarım
Thermal stability needs to start from antioxidants and temperature control
thermal stabilityantioxidantdegradationtemperature