Processing Machinery
7 visualizações
Poor thermal stability of styrene-butadiene transparent resin (K resin) during processing
Fenómeno do problema
Styrene-butadiene transparent resin (K resin) has poor thermal stability during processing; performance decreases significantly after repeated processing, with severe degradation
Análise das causas
Insufficient antioxidant addition or improper type
Processing temperature too high (exceeding the 200-240°C upper limit) accelerates degradation
Excessive screw shear accelerates thermo-oxidative degradation
Regrind ratio too high, degradation accumulates
Antioxidants fail at high temperature
Solução
Increase antioxidant addition amount
Reduce processing temperature to a reasonable value of 200-240°C
Reduce screw rotation speed to reduce shear
Reduce regrind ratio ≤15%
Select antioxidants with good high-temperature stability
Conclusão principal
Thermal stability needs to start from antioxidants and temperature control