Blow Molding 7 görüntüleme

Uneven wall thickness of blow molded containers

Sorun Belirtisi
Wall thickness of blow molded containers is uneven, some parts too thin or too thick, affecting use strength and appearance
Neden Analizi
Uneven parison wall thickness Uneven blowing pressure distribution Improper mold cavity design Uneven parison temperature Blow-up ratio too large, local over-stretching
Çözüm
Optimize parison wall thickness control (wall thickness controller) Adjust blowing pressure and blowing time Optimize mold cavity design Control uniform parison temperature Reasonably design the blow-up ratio
Temel Çıkarım
2079851475616104457 wall thickness needs to start from parison and blowing
2079851475616104457 wall thicknessparison controlblowing pressure

Bu faydalı oldu mu?

0 kişi bunu faydalı buldu