Blow Molding 5 Aufrufe

Uneven wall thickness of blow molded containers

Problembeschreibung
Wall thickness of blow molded containers is uneven, some parts too thin or too thick, affecting use strength and appearance
Ursachenanalyse
Uneven parison wall thickness Uneven blowing pressure distribution Improper mold cavity design Uneven parison temperature Blow-up ratio too large, local over-stretching
Lösung
Optimize parison wall thickness control (wall thickness controller) Adjust blowing pressure and blowing time Optimize mold cavity design Control uniform parison temperature Reasonably design the blow-up ratio
Wichtigste Erkenntnis
2079851475616104457 wall thickness needs to start from parison and blowing
2079851475616104457 wall thicknessparison controlblowing pressure