Blow Molding 7 Aufrufe

Deformation of blow molded containers after demolding

Problembeschreibung
Blow molded containers deform after demolding, shape does not match the design, bottom or side walls warp
Ursachenanalyse
Insufficient cooling time, container rigidity not established Mold temperature too high (exceeding the 20-50°C upper limit), slow cooling Insufficient blowing pressure, parison not fully attached to the mold wall Parison temperature too high, insufficient rigidity Improper demolding timing
Lösung
Extend cooling time Reduce mold temperature to the lower value of 20-50°C Increase blowing pressure Appropriately reduce parison temperature Ensure demolding after complete cooling
Wichtigste Erkenntnis
2079851475616104457 deformation needs to start from cooling and blowing
2079851475616104457 deformationcoolingblowing pressure