Blow Molding 7 Aufrufe

Poor wall thickness control accuracy of K-RESIN blow molded containers

Problembeschreibung
Wall thickness control accuracy of K-RESIN blow molded containers is poor, locally too thin or too thick
Ursachenanalyse
Low K-RESIN parison viscosity, fast sag, uneven wall thickness Difficult parison temperature control Improper blow-up ratio design Improper wall thickness controller parameter settings K-RESIN rubber component causes parison elasticity differences
Lösung
Reduce parison temperature to reduce sag Precisely control parison temperature Reasonably design the blow-up ratio Optimize wall thickness controller parameters Use K-RESIN elastic characteristics to adjust the blowing strategy
Wichtigste Erkenntnis
K-RESIN '2079851475616104457 needs precise control of parison temperature and blow-up ratio
K resin'2079851475616104457 wall thicknessparison sag