Sorun Belirtisi
After color change, the previous color still remains after multiple injections
Neden Analizi
Previous color material remains in the screw and barrel; accumulated material in dead zones is not completely removed; purging time is insufficient
Çözüm
Use high-viscosity purging material of the same matrix for color change; the temperature-difference purging method of heating up then cooling down; disassemble the screw and nozzle for thorough cleaning if necessary
Temel Çıkarım
Thorough color change is necessary for multi-variety small-batch production
color changecross-contaminationpurging materialtemperature-difference purgingdead zone