Injection Molding 8 görüntüleme

Severe mold gate wear

Sorun Belirtisi
The gate dimension obviously enlarges after thousands of injection shots
Neden Analizi
High-concentration glass fiber melt repeatedly scours the gate at high speed, producing abrasive erosion; the gate design size is too small, causing extremely high local flow velocity and shear stress
Çözüm
Use hard alloy (such as SKD11 or higher) to make gate inserts; appropriately increase the gate size to reduce flow velocity (gate ≥60% of wall thickness); streamlined design of the gate transition section
Temel Çıkarım
The gate is the weakest link most prone to wear in LGFPP molds
gate wearhard alloySKD11gate sizeabrasion

Bu faydalı oldu mu?

0 kişi bunu faydalı buldu

ChemAI