Injection Molding 11 visualizaciones

Severe mold gate wear

Fenómeno del problema
The gate dimension obviously enlarges after thousands of injection shots
Análisis de la causa
High-concentration glass fiber melt repeatedly scours the gate at high speed, producing abrasive erosion; the gate design size is too small, causing extremely high local flow velocity and shear stress
Solución
Use hard alloy (such as SKD11 or higher) to make gate inserts; appropriately increase the gate size to reduce flow velocity (gate ≥60% of wall thickness); streamlined design of the gate transition section
Conclusión clave
The gate is the weakest link most prone to wear in LGFPP molds
gate wearhard alloySKD11gate sizeabrasion