Molds & Tooling 6 görüntüleme

Product shrinkage rate high and fluctuating

Sorun Belirtisi
Large dimensional deviations, with shrinkage rate fluctuating irregularly between 1.2-1.8%
Neden Analizi
Inconsistent cooling rates in different areas cause crystallinity differences; mold temperature fluctuations cause shrinkage rate changes; inconsistent holding switchover timing
Çözüm
Stabilize the mold temperature at 180-200°C±2°C; finely adjust the holding switchover point and holding pressure curve; ensure sufficient cooling time
Temel Çıkarım
PEEK shrinkage rate is highly sensitive to mold temperature and cooling rate
shrinkage ratecrystallinity differencemold temperatureholding pressure curvecooling time

Bu faydalı oldu mu?

0 kişi bunu faydalı buldu

ChemAI