Molds & Tooling 2 مشاهدة

ABS brittle cracking——sharp corner and notch stress concentration

ظاهرة المشكلة
The product cracks in batches at sharp corners, notches, or sudden wall thickness changes.
تحليل الأسباب
Sharp corners and notches cause stress concentration during filling and cooling; the internal stress cannot be released, and cracking occurs along the sharp corners during use or after demolding.
الحل
①Change sharp corners to rounded corners, minimum corner radius 0.5mm; ②make the wall thickness as uniform as possible, set gradual transition sections for thick-thin transitions; ③add reinforcing ribs in the transition area when necessary.
الخلاصة الأساسية
A sharp corner in the structure is the starting point of a crack.
ABS;stress concentration;sharp corner;rounded corner;structural design