ظاهرة المشكلة
ASA extrusion grade shrinkage 0.5-0.9%, injection grade 0.4-0.7%.
تحليل الأسباب
ASA extrusion grade linear mold shrinkage 0.5-0.9%; injection grade 0.4-0.7%; grade differences; process influence; mold design; dimension management.
الحل
①Design according to grade shrinkage; ②extrusion injection differences; ③process stability; ④dimension verification; ⑤mold compensation.; After adjustment, continuously sample to verify the effect, and resume mass production after confirming stability