Extrusion & Post
8 visualizações
ASA shrinkage 0.5-0.9
Fenómeno do problema
ASA extrusion grade shrinkage 0.5-0.9%, injection grade 0.4-0.7%.
Análise das causas
ASA extrusion grade linear mold shrinkage 0.5-0.9%; injection grade 0.4-0.7%; grade differences; process influence; mold design; dimension management.
Solução
①Design according to grade shrinkage; ②extrusion injection differences; ③process stability; ④dimension verification; ⑤mold compensation.; After adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Conclusão principal
ASA shrinkage grade differences are the design basis; process stability ensures consistency; verification ensures accuracy.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence