Extrusion & Post 6 مشاهدة

EVA Film High Shrinkage Rate

ظاهرة المشكلة
Film shrinkage after lamination causes cell displacement or microcracks.
تحليل الأسباب
The film itself has a high shrinkage rate or the lamination process does not match; differences in shrinkage characteristics of different batches of film also cause fluctuations.; During on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
الحل
①Select a low-shrinkage film; ②optimize the lamination temperature curve; ③test the shrinkage rate of incoming materials by batch; ④fine-tune the lamination process with the batch.; After adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
الخلاصة الأساسية
Film shrinkage affects module reliability; low-shrinkage material plus process matching is the solution.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
EVA; film; shrinkage; cells; lamination; batch