Molding Process 6 مشاهدة

Dielectric Advantages and Molding Requirements of LCP in 5G High-Frequency Applications

ظاهرة المشكلة
【Problem Phenomenon】When LCP is used for 5G antennas and high-frequency connectors, molding fluctuations cause dielectric consistency to fall below standard
تحليل الأسباب
LCP's dielectric loss is as low as about 0.002 and stable with frequency, making it an ideal material for 5G high frequency; but orientation differences cause dielectric anisotropy, and molding fluctuations affect batch consistency; Ringier literature records its dielectric characteristics and molding difficulties
الحل
For high-frequency parts, solidify orientation-related process parameters: lock gate, injection speed and mold temperature; sample-inspect incoming dielectric batches; link key dimensions and dielectric performance in SPC; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
الخلاصة الأساسية
LCP for 5G wins on dielectric; batch consistency relies on process locking and SPC; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
5G dielectric loss high frequency consistency