Injection Molding 8 مشاهدة

PA6 '2079851475616104452 Metering Fluctuation

ظاهرة المشكلة
Cushion fluctuation and unstable weight, short shots and flash alternating.
تحليل الأسباب
PA6 solidifies quickly, and slight leakage of the check ring affects metering; unstable feeding also does; low-viscosity material has high requirements for check ring sealing; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
الحل
①Disassemble and check the wear and sealing of the check ring, and replace it when necessary;②check hopper feeding and throat cooling to ensure stable and smooth feeding;③stabilize the back pressure setting to ensure consistency of plasticization and metering;④continuously monitor cushion fluctuation as an early warning of metering stability;⑤clean the screw head.
الخلاصة الأساسية
Stable PA6 metering = 'check ring health': low-viscosity nylon has extremely high requirements for check ring sealing; cushion fluctuation is the most intuitive alarm; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence.
PA6; metering fluctuation; check ring; cushion