Molds & Tooling 5 مشاهدة

PA6 and PA66 Selection

ظاهرة المشكلة
Short shots after switching to PA66 with the same mold, or complaints about PA6 parts softening and deforming in high-temperature environments
تحليل الأسباب
PA66's melting point of 260°C is 40°C higher than PA6, requiring a melt temperature of 270-300°C and a higher mold temperature; directly processing PA66 with the PA6 process inevitably results in poor plasticization, and the reverse results in degradation
الحل
①Set process windows separately according to the melting point difference; ②select PA66 for long-term working environments above 120°C; ③select PA6 for cost-sensitive scenarios where the temperature does not exceed 80°C
الخلاصة الأساسية
PA6 and PA66 processes cannot be borrowed from each other; temperature rating and cost are the two dimensions of selection, and changing material must change the entire set of process parameters; after confirming effectiveness, fix the parameters and practices into the work instructions to prevent recurrence
PA6;PA66;selection;melting point difference;process window