Extrusion & Post 13 مشاهدة

PVB Ink Adhesion

ظاهرة المشكلة
PVB laminated glass ceramic ink area adhesion is poor, bubbles and delamination.
تحليل الأسباب
Ceramic ink compatibility with glass/PVB; ink curing degree; surface energy differences; ink thickness uniformity.; When troubleshooting on site, verify item by item according to this mechanism, avoiding blind machine adjustment based only on experience
الحل
①Ink compatibility verification; ②Curing process specification; ③Ink thickness control; ④Adhesion testing.; After adjustment, continuously sample to verify the effect, confirm stability before resuming mass production
الخلاصة الأساسية
Adhesion in PVB ink areas is a special challenge; compatibility is a material issue; testing and verification are indispensable.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PVB;ink;adhesion;compatibility;curing;testing