Extrusion & Post
10 visualizaciones
PVB Ink Adhesion
Fenómeno del problema
PVB laminated glass ceramic ink area adhesion is poor, bubbles and delamination.
Análisis de la causa
Ceramic ink compatibility with glass/PVB; ink curing degree; surface energy differences; ink thickness uniformity.; When troubleshooting on site, verify item by item according to this mechanism, avoiding blind machine adjustment based only on experience
Solución
①Ink compatibility verification; ②Curing process specification; ③Ink thickness control; ④Adhesion testing.; After adjustment, continuously sample to verify the effect, confirm stability before resuming mass production
Conclusión clave
Adhesion in PVB ink areas is a special challenge; compatibility is a material issue; testing and verification are indispensable.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence