TPE Product Mold Temperature Selection
ظاهرة المشكلة
The mold temperature is difficult to decide between high and low.
تحليل الأسباب
High mold temperature gives good gloss but a long cycle; low mold temperature is fast but the surface is poor.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience; this mechanism has been repeatedly verified by industry information and should be confirmed first during troubleshooting
الحل
①Select the range according to product requirements; ②Take the upper limit for appearance parts; ③Stabilize the mold temperature; ④Record and verify.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
الخلاصة الأساسية
Mold temperature is the balance between quality and efficiency.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا
شكرًا لك على ملاحظاتك!