Extrusion & Post
13 مشاهدة
TPE Extrusion Temperature
ظاهرة المشكلة
The TPE extrusion surface is rough and the melt is unstable
تحليل الأسباب
The extrusion temperature fluctuates or is too low; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience; this mechanism has been repeatedly verified by industry information and should be confirmed first during troubleshooting
الحل
Stably control the extrusion temperature at 170-210℃; uniform die temperature; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
الخلاصة الأساسية
TPE extrusion temperature stability comes first; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا