Extrusion & Post 10 visualizaciones

TPE Extrusion Temperature

Fenómeno del problema
The TPE extrusion surface is rough and the melt is unstable
Análisis de la causa
The extrusion temperature fluctuates or is too low; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience; this mechanism has been repeatedly verified by industry information and should be confirmed first during troubleshooting
Solución
Stably control the extrusion temperature at 170-210℃; uniform die temperature; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Conclusión clave
TPE extrusion temperature stability comes first; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
TPE extrusion temperature roughness stability