Injection Molding
8 مشاهدة
Obvious EAA surface color difference
ظاهرة المشكلة
Different shades of color in different parts of EAA products, color difference ΔE>5
تحليل الأسباب
Uneven dispersion of color masterbatch; pigment orientation during injection causing uneven color distribution; barrel temperature fluctuation causing color change
الحل
1) Use the color masterbatch masterbatch method to ensure uniform dispersion; 2) Reduce injection speed to reduce pigment orientation; 3) Stabilize barrel temperature to ±2°C
الخلاصة الأساسية
Color difference is caused by uneven dispersion and orientation; masterbatch method and stable processing are key
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا
شكرًا لك على ملاحظاتك!