Injection Molding 4 views

Obvious EAA surface color difference

Problem Phenomenon
Different shades of color in different parts of EAA products, color difference ΔE>5
Cause Analysis
Uneven dispersion of color masterbatch; pigment orientation during injection causing uneven color distribution; barrel temperature fluctuation causing color change
Solution
1) Use the color masterbatch masterbatch method to ensure uniform dispersion; 2) Reduce injection speed to reduce pigment orientation; 3) Stabilize barrel temperature to ±2°C
Key Takeaway
Color difference is caused by uneven dispersion and orientation; masterbatch method and stable processing are key
EAAcolor differencecolor masterbatch dispersionpigment orientationtemperature stability