Production & Quality
13 مشاهدة
Poor EMA fatigue resistance
ظاهرة المشكلة
EMA product fatigue life <10⁴ cycles, below the 10⁵ cycles requirement
تحليل الأسباب
EMA elastic recovery insufficient, accumulating plastic deformation each cycle; crosslinking degree too low with fast fatigue crack growth
الحل
1) Increase crosslinking degree to improve recovery and reduce accumulated deformation; 2) Select high molecular weight grade to raise fatigue threshold; 3) Product design reduces stress concentration
الخلاصة الأساسية
Poor fatigue resistance is caused by insufficient recovery and fast crack growth; increasing crosslinking is key
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا
شكرًا لك على ملاحظاتك!