Material Analysis
7 مشاهدة
PU hardness too high
ظاهرة المشكلة
PU product Shore hardness 5-10 degrees higher than target, hard to touch
تحليل الأسباب
PU crystallinity too high, rigidity increased; too much filler added; cooling too fast, crystallization imperfect but rigidity frozen
الحل
1) Reduce cooling rate to make crystallization complete and reduce hardness feel; 2) Reduce filler addition; 3) Add plasticizer 0.5wt% to reduce hardness
الخلاصة الأساسية
High hardness is caused by crystallization and filler; adjusting cooling and filler are key