Material Analysis
8 visualizaciones
PU hardness too high
Fenómeno del problema
PU product Shore hardness 5-10 degrees higher than target, hard to touch
Análisis de la causa
PU crystallinity too high, rigidity increased; too much filler added; cooling too fast, crystallization imperfect but rigidity frozen
Solución
1) Reduce cooling rate to make crystallization complete and reduce hardness feel; 2) Reduce filler addition; 3) Add plasticizer 0.5wt% to reduce hardness
Conclusión clave
High hardness is caused by crystallization and filler; adjusting cooling and filler are key
¿Le ha resultado útil?
0 personas encontraron esto útil
¡Gracias por sus comentarios!