Injection Molding 7 مشاهدة

Warpage in PVA '2079851475616104452

ظاهرة المشكلة
After demolding, PVA injection molded products warp 2-3mm/100mm, flatness not up to standard
تحليل الأسباب
PVA shrinkage large and mold temperature uneven, causing directional shrinkage differences; gate position improper, flow orientation stress released unevenly; cooling time insufficient
الحل
1) Increase mold temperature to 40-60°C to reduce temperature difference; 2) Increase holding pressure to 50-70MPa; 3) Optimize gate position for uniform flow; 4) Extend cooling time; 5) Annealing treatment to release residual stress
الخلاصة الأساسية
Warpage is caused by shrinkage difference and orientation stress; uniform mold temperature and holding are key
PVA injection warpage shrinkage holding pressure annealing treatment