Product partially not filled

ظاهرة المشكلة
The product is partially not filled, the edges are incomplete, especially obvious in thin-walled areas, the surface at the unfilled area is rough and without gloss
تحليل الأسباب
Injection pressure insufficient or injection speed too slow Barrel temperature low (below the lower limit of 170-230°C), poor fluidity Poor mold venting, large cavity pressure loss Gate too small or runner too long, large resistance Product wall thickness too thin, melt difficult to reach the end
الحل
Increase injection pressure and injection speed Appropriately increase the barrel temperature to the 170-230°C range Improve mold venting Increase gate and runner dimensions Appropriately increase wall thickness or increase the number of gates
الخلاصة الأساسية
Short shot needs to be addressed from pressure, temperature, venting, and gate
material shortageshort shotinjection pressurefluidity