Injection Molding 7 visualizaciones

Product partially not filled

Fenómeno del problema
The product is partially not filled, the edges are incomplete, especially obvious in thin-walled areas, the surface at the unfilled area is rough and without gloss
Análisis de la causa
Injection pressure insufficient or injection speed too slow Barrel temperature low (below the lower limit of 170-230°C), poor fluidity Poor mold venting, large cavity pressure loss Gate too small or runner too long, large resistance Product wall thickness too thin, melt difficult to reach the end
Solución
Increase injection pressure and injection speed Appropriately increase the barrel temperature to the 170-230°C range Improve mold venting Increase gate and runner dimensions Appropriately increase wall thickness or increase the number of gates
Conclusión clave
Short shot needs to be addressed from pressure, temperature, venting, and gate